MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexBond™ ST1150 50 MIL Foaming Adhesive Film
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Foaming core splice adhesive. It is especially useful in bonding sections and edge filling honeycomb. It is ideal for use in thick sections of honeycomb.

Features:

  • Cure from 120oC/248oF to 180oC/356oF
  • Low volatiles content: = 1% (after cure 1h at 178oC/325oF - 3oC/min)
  • Shelf-life: 1 year at temperature = -18oC/0oF + 15 days at room temperature (= 23oC/73oF)
Applications:
  • Core splice bonding
  • Sandwich construction

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength  7.50 MPa
@Temperature 80.0 °C
1090 psi
@Temperature 176 °F
Lap Shear, Curing 1h 120°C; EN2267-2
 7.50 MPa
@Temperature 22.8 °C
1090 psi
@Temperature 73.0 °F
Lap Shear, Curing 1h 120°C, Wet ageing: 70°C, 85% relative humidity, saturation; EN2267-2
 8.00 MPa
@Temperature 22.8 °C
1160 psi
@Temperature 73.0 °F
Lap Shear, Curing 1h 120°C; EN2267-2
 8.00 MPa
@Temperature 80.0 °C
1160 psi
@Temperature 176 °F
Lap Shear, Curing 1h 175°C; EN2267-2
 8.00 MPa
@Temperature 22.8 °C
1160 psi
@Temperature 73.0 °F
Lap Shear, Curing 1h 175°C, Wet ageing: 70°C, 85% relative humidity, saturation; EN2267-2
 8.50 MPa
@Temperature 22.8 °C
1230 psi
@Temperature 73.0 °F
Lap Shear, Curing 1h 175°C; EN2267-2
 10.0 MPa
@Temperature -55.0 °C
1450 psi
@Temperature -67.0 °F
Lap Shear, Curing 1h 120°C; EN2267-2
 10.0 MPa
@Temperature -55.0 °C
1450 psi
@Temperature -67.0 °F
Lap Shear, Curing 1h 175°C; EN2267-2
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature <=-18.0 °C
12.0 Month
@Temperature <=-0.400 °F
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9300 / 322456

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.