MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics TufFlex™ GF 1831 PVC/Nitrile Alloy
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Application: High Grade Oil Resistant PVC/Nitrile Soling Material with excellent Abrasion and slip resistant properties designed for work boot applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858Instant; ASTM D2240
 50
@Time 15.0 sec
50
@Time 0.00417 hour
ASTM D2240
Tensile Strength 8.48 MPa1230 psiASTM D412
Elongation at Break 575 %575 %ASTM D412
Coefficient of Friction 0.610.61Varnished Wood: Wet; ASTM D1894
 0.610.61Mason Tiles: Wet; ASTM D1894
 0.770.77Mason Tiles: Dry; ASTM D1894
 0.820.82Vinyl Tiles: Wet; ASTM D1894
 0.910.91Varnished Wood: Dry; ASTM D1894
 1.071.07Vinyl Tiles: Dry; ASTM D1894
Abrasion 200200[%], NBS; ASTM D297
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -42.0 °C-43.6 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 182 °C350 - 360 °FSuggested Stock
 
Descriptive Properties
Rossflex50000-20°F, ASTM D1052

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aurora Plastics GE-960F PVC/Nitrile Alloy
Aurora Plastics TufFlex™ GF 1815 PVC/Nitrile Alloy
Avient Elastamax™ XL-0255-1 PVC/Nitrile-Based Thermoplastic Elastomer
Global Atron Nylon 6 UIM 33 GF Nylon 6 33% Glass Filled, Impact Modified Black
Daicel CEVIAN® S5230 30% GF PC/ABS alloy

PSEPN012 / 179016

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.