System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC VALOX™ V3004 PBT (Asia)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.29
g/cc
1.29
g/cc
ASTM D792
Density
1.29
g/cc
0.0466
lb/in³
ISO 1183
Water Absorption
0.20 %
0.20 %
23°C/sat; ISO 62
Moisture Absorption
0.0800 %
0.0800 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.021
-
0.027
cm/cm
@Thickness 3.20 mm
0.021
-
0.027
in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse
0.021
-
0.027
cm/cm
@Thickness 3.20 mm
0.021
-
0.027
in/in
@Thickness 0.126 in
SABIC method
Melt Flow
21
g/10 min
@Load 2.16 kg,
Temperature 250 °C
21
g/10 min
@Load 4.76 lb,
Temperature 482 °F
cm³/10 min; ISO 1133
23
g/10 min
@Load 2.16 kg,
Temperature 250 °C
23
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
22.0
MPa
3190
psi
50 mm/min; ASTM D638
30.0
MPa
4350
psi
50 mm/min; ISO 527
Tensile Strength, Yield
50.0
MPa
7250
psi
50 mm/min; ISO 527
51.0
MPa
7400
psi
50 mm/min; ASTM D638
Elongation at Break
200 %
200 %
50 mm/min; ISO 527
300 %
300 %
50 mm/min; ASTM D638
Elongation at Yield
3.7 %
3.7 %
50 mm/min; ISO 527
4.0 %
4.0 %
50 mm/min; ASTM D638
Tensile Modulus
2.35
GPa
341
ksi
1mm/min; ISO 527
2.40
GPa
348
ksi
50 mm/min; ASTM D638
Flexural Yield Strength
74.0
MPa
10700
psi
2 mm/min; ISO 178
82.0
MPa
11900
psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2.10
GPa
305
ksi
2 mm/min; ISO 178
2.30
GPa
334
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched
0.510
J/cm
0.955
ft-lb/in
ASTM D256
0.450
J/cm
@Temperature -30.0 °C
0.843
ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO)
6.00
kJ/m²
2.86
ft-lb/in²
80*10*4; ISO 180/1A
4.00
kJ/m²
@Temperature -30.0 °C
1.90
ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched
0.700
J/cm²
3.33
ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
60.0
J
44.3
ft-lb
ASTM D3763
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
91.8
µm/m-°C
@Temperature -40.0 - 40.0 °C
51.0
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
91.8
µm/m-°C
@Temperature -40.0 - 40.0 °C
51.0
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow
75.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
75.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
120
°C
@Thickness 3.20 mm
248
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
48.0
°C
118
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
52.0
°C
@Thickness 3.20 mm
126
°F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point
165
°C
329
°F
Rate B/50; ISO 306
167
°C
333
°F
Rate B/50; ASTM D1525
170
°C
338
°F
Rate B/120; ISO 306
Processing Properties
Metric
English
Comments
Nozzle Temperature
245
-
260
°C
473
-
500
°F
Injection Molding
Zone 1
240
-
255
°C
464
-
491
°F
Zone 2
245
-
260
°C
473
-
500
°F
Zone 3
250
-
265
°C
482
-
509
°F
Melt Temperature
250
-
265
°C
482
-
509
°F
Mold Temperature
50.0
-
75.0
°C
122
-
167
°F
Drying Temperature
120
°C
248
°F
Injection Molding
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Injection Molding
12.0
hour
12.0
hour
Cumulative; Injection Molding
Moisture Content
0.020 %
0.020 %
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Shot Size
40 - 80 %
40 - 80 %
Vent Depth
0.00250
-
0.00380
cm
0.000984
-
0.00150
in
Screw Speed
50
-
100
rpm
50
-
100
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABI10298 / 243765
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.