MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips MC6560 Rubber Modified Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description

Chevron MC6560 is a high impact polystyrene injection molding material with well-balanced flow and set-up time and good resistance to heat distortion. It also has good impact strength at low temperatures and excellent chemical resistance. Chevron MC6560 natural complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods.

Applications

Chevron MC6560 is recommended for moldings with medium- to heavy-walled sections such as furniture, refrigerator breaker trim, housewares and appliances.Information provided by Chevron Phillips Chemical Company.

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Melt Flow 4.0 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3800 psiASTM D638
Tensile Strength, Yield 4200 psiASTM D638
Elongation at Break 50 %ASTM D638
Tensile Modulus 300000 psiASTM D638
Flexural Strength 6600 psiASTM D790B
Flexural Modulus 310000 psiASTM D790B
Izod Impact, Notched 1.60 ft-lb/in1/4 in.; ASTM D256
 2.40 ft-lb/in1/8 in.; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 182 °FASTM D648
Vicat Softening Point 210 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe)
Trinseo Magnum™ 344CC ABS
RTP Company RTP 699 X 147364 Acrylonitrile Butadiene Styrene (ABS); ESD Protection - Permanently Static Dissipative - UV Stabilized - Preliminary Datasheet
RTP Company RTP 699 X 141354 Acrylonitrile Butadiene Styrene (ABS); Permanently Anti-static - ESD Protection

PPSRA23 / 58253

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.