MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.

Features: Excellent combination of sealability, mechanical strength and optics.

Applications: Sealing layer in coextruded films principally for food packaging, heavy duty shipping sacks, and general purpose film

FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2a.

Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.

Information provided by Huntsman Corporation

Key Words: Linear Low Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D1505
Thickness 1.00 mil
Melt Flow 1.1 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 690 %ASTM D882
Film Elongation at Break, TD >= 700 %ASTM D882
Secant Modulus, MD 0.172 GPaASTM D882
Secant Modulus, TD 0.186 GPaASTM D882
Elmendorf Tear Strength MD 460 gASTM D1922
Elmendorf Tear Strength TD 950 gASTM D1922
Elmendorf Tear Strength, MD 460 g/milASTM D1922
Elmendorf Tear Strength, TD 950 g/milASTM D1922
Dart Drop 290 g/milASTM D1709
Dart Drop Test 290 gASTM D1709
Film Tensile Strength at Break, MD 40.0 MPaASTM D882
Film Tensile Strength at Break, TD >= 19.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %ASTM D1003
Gloss 66 %at 45°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 - 245 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHUP51 / 47860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.