MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Brewer Science BrewerBOND® 305 Temporary Bonding Material
Categories: Other Engineering Material

Material Notes: BrewerBOND® 305 temporary wafer bonding material is an organic coating that enables back-end-of-line (BEOL) processing of ultrathin wafers using standard semiconductor equipment. This product improves throughput, simplifies cleaning, and shortens processing time.

BrewerBOND® 305 material is an organic temporary bonding material that improves throughput, simplifies cleaning, and shortens processing time. The material is stable in back-end-of-line processing up to 300°C (depending on downstream process specifications). Debonding is efficient and can be done in two ways. The first method is laser debonding with no force. The second method is mechanical debonding at room temperature with low force. This debonding versatility makes BrewerBOND® 305 material a great option for many different wafer-processing needs.

Market sectors include 3-D wafer-level packaging; MEMS; and Compound semiconductor.

Benefits:

  • Enables backside temperature processing at 250°C - 300°C
  • Enables mechanical or laser debonding with low force
  • Maximizes wafer yield with optimized temporary wafer bonding with mechanical or laser debonding process
  • Post-bond TTV < 2 µm
  • Reduced cleaning chemical consumption and time

Information provided by Brewer Science.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 600000 cP
@Temperature 300 °C
Complex Melt Viscosity
 6.00e+6 cP
@Temperature 200 °C
Complex Melt Viscosity
 3.00e+7 cP
@Temperature 150 °C
Complex Melt Viscosity
 1.00e+10 cP
@Temperature 50.0 °C
Complex Melt Viscosity
Brookfield Viscosity 3300 cP
@Temperature 37.8 °C
BrewerBOND® 305-30
 5470 cP
@Temperature 25.0 °C
BrewerBOND® 305-30
 6700 cP
@Temperature 37.8 °C
BrewerBOND® 305
 12825 cP
@Temperature 25.0 °C
BrewerBOND® 305
Thickness 16.0 micronsBrewerBOND® 305-30; Spin Speed 1700 rpm
 28.0 micronsBrewerBOND® 305; Spin Speed 1700 rpm
 30.0 micronsBrewerBOND® 305-30; Spin Speed 900 rpm
 55.0 micronsBrewerBOND® 305; Spin Speed 900 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brewer Science WaferBOND HT-10.10 Temporary Bonding Material
Brewer Science WaferBOND CR-220 Temporary Bonding Material
Brewer Science ProTEK® PSB Photosensitive Protective Coating
Brewer Science ProTEK® B3 Alkaline-Resistant Coating
Brewer Science BrewerBOND® 701 Laser Release Material

PBREW991 / 193507

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.