MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SYNTHOS Kralex® 1500 Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: KRALEX® 1500 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin acids and contains 23.5% of chemically bonded styrene. It is coagulated by a system of acid and organic coagulant, does not contain extender oil and is stabilized by staining antioxidant.

KRALEX® 1500 is appropriate for rubber compounds used in the production of car tires and inner tubes, conveyor belts, footwear, cables, hosepipes and various technical rubber articles.
It is not approved for production of rubber articles coming into contact with foods or drinking water.
Synthos was formerly known as Kaucuk.

Synthos was formerly known as Kaucuk. All information provided by Synthos.

Key Words: SBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Mooney Viscosity 44 - 54
@Temperature 100 °C
44 - 54
@Temperature 212 °F
(1+4); ASTM D1646
Ash <= 0.40 %<= 0.40 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Acid Value 5.0 - 7.55.0 - 7.5ASTM D5774
Styrene Content 23.5 %23.5 %ASTM D5775
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 23.0 MPa3340 psi35'/145°C; ASTM D412
Elongation at Break 400 %400 %35'/145°C; ASTM D412
300% Modulus 13.0 - 19.0 MPa
@Strain 300 %
1890 - 2760 psi
@Strain 300 %
35'/145°C; ASTM D412
 
Descriptive Properties
50% of Vulcanization t' 50 (min.)6.5-10.5ASTM D5289
Antioxidant GradeStaining
Compound Safety ts 1 (min.)2.2-4.0ASTM D5289
Maximal Moment (dNm)19-22ASTM D5289
Minimal Moment (dNm)2.1-2.8ASTM D5289
Optimal Vulcanization t' 90 (min.)12-17ASTM D5289
Soaps content (%)<= 0.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock 60 SBR Sheet Rubber
LG Chemical Lutex 703 SBR Latex
KKPC KOSYN SOL 5740 Solution Styrene Butadiene Rubber (S-SBR)
KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR)
KKPC KOSYN SOL 5001 Solution Styrene Butadiene Rubber (S-SBR)

PSYNT001 / 82614

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.