MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont™ 5069 Silver Conductor
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: DuPont 5069 is a water-based Silver Conductor designed for Flexographic and Gravure printing, or for Spraying. The 5069 meets low Volatile Organic Compound (VOC) requirements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/cc
Solids Content 46 - 51 %
Filler Content 0.00 %Silver (Ag)
Particle Size 1.0 µm
Viscosity 23 - 33 cP
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.40 - 0.45 ohm
 
Processing PropertiesOriginal ValueComments
Cure Time 120 - 300 sec
 
Descriptive Properties
Binder SystemProprietary
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester, Polyimide, Paper, Epoxy Glass
Solvent SystemWater and BCA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2040226D4 Curable Carbon Ink
Parker Chomerics CHO-FLEX 4430 Conductive Polyester Ink
NuSil R-1008 Silicone Ink
NuSil MED8-6608-2 Ink - Restricted Medical Use
NovaCentrix PSI-211® Conductive Screen Ink

PFLEXCM28 / 179430

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.