MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes:
  • Electrical Conductivity
  • Increase At Corrosion Resistance
  • Increase In Deformation Strength Against Load
  • Decrease In Thermal Expansion
  • High Resistance Against Acids
  • Ease of Mechanical Processing
  • Stretching
  • Resistance Against Stroke
  • Increase In Thermal Conductivity

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.80 - 4.00 g/ccASTM D1457-18
Deformation 5.0 - 5.5 %230°C, 1 day, 140 kg/cm^2; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63 - 70ASTM D2240
Tensile Strength, Yield 170 - 175 kg(f)/cm²ASTM D1708
Elongation at Break 170 - 180 %ASTM D1708
Izod Impact, Notched 11.0 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM E831
Thermal Conductivity 0.0023055 cal cm/sec-cm²-°CASTM C177
 
Descriptive Properties
Corrosion10 - 15 cc-dak/kg-ms25 - 1000°C
Kinding Temperature640°C, ASTM D1929

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze
Murtfeldt Murflor® Polytetrafluoroethylene
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon
AGC Fluon® RB2515 15% Carbon Fiber, PTFE Filled Compound

PPOLIM03 / 56969

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.