MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Notes: Elexar® EL-8421 is a high performance thermoplastic elastomer designed for the electrical applications requiring flexibility over a wide temperature range. Elexar® EL-8421 is a high durometer that is RoHS and REACH SVHC compliant. This grade is UL listed and is suitable for both injection molding and extrusion.

Features: Good Colorability; Halogen Free; Heat Aging Resistant; High Hardness; High Tensile Strength; Medium Density; Medium Flow

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D792
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 200 °C
16 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength, Yield 20.0 MPa2900 psi0.02 in, Die C, 20 in/min, die cut from extruded tapes; ASTM D412
 8.00 MPa
@Treatment Temp. 121 °C,
Time 64800 sec
1160 psi
@Treatment Temp. 250 °F,
Time 18.0 hour
in Vegetable Oil; ASTM D471
 14.0 MPa
@Treatment Temp. 121 °C,
Time 64800 sec
2030 psi
@Treatment Temp. 250 °F,
Time 18.0 hour
in Animal Fat; ASTM D471
 20.0 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
2900 psi
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
 21.39 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
3103 psi
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
Tensile Stress at Strain  6.58 MPa
@Strain 100 %,
Thickness 0.508 mm
955 psi
@Strain 100 %,
Thickness 0.0200 in
Die C, 20 in/min, die cut from extruded tapes; ASTM D412
 8.62 MPa
@Strain 300 %,
Thickness 0.508 mm
1250 psi
@Strain 300 %,
Thickness 0.0200 in
Die C, 20 in/min, die cut from extruded tapes; ASTM D412
Elongation at Break 630 %630 %0.02 in, Die C, 20 in/min, die cut from extruded tapes; ASTM D412
 441 %
@Treatment Temp. 121 °C,
Time 64800 sec
441 %
@Treatment Temp. 250 °F,
Time 18.0 hour
in Vegetable Oil; ASTM D471
 472.5 %
@Treatment Temp. 121 °C,
Time 64800 sec
472.5 %
@Treatment Temp. 250 °F,
Time 18.0 hour
in Animal Fat; ASTM D471
 573.3 %
@Treatment Temp. 136 °C,
Time 605000 sec
573.3 %
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
 655.2 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
655.2 %
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.50e+16 ohm-cm
@Temperature 50.0 °C
3.50e+16 ohm-cm
@Temperature 122 °F
ASTM D257
Insulation Resistance 9.00e+10 ohm9.00e+10 ohmIEC 60167
Dielectric Constant 2.4
@Frequency 1000 Hz
2.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 38.2 kV/mm970 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FContinuous; UL-1581
Brittleness Temperature -65.6 °C-86.1 °FASTM D746
UL RTI, Electrical 50.0 °C122 °FUL746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL746
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
All Colors
Oxygen Index 18 %18 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 199 - 216 °C390 - 420 °F
Middle Barrel Temperature 213 - 221 °C415 - 430 °F
Front Barrel Temperature 221 - 227 °C430 - 440 °F
Nozzle Temperature 221 - 229 °C430 - 445 °F
Zone 1 193 - 210 °C380 - 410 °F
Zone 2 199 - 216 °C390 - 420 °F
Zone 3 213 - 221 °C415 - 430 °F
Zone 4 221 - 227 °C430 - 440 °F
Zone 5 221 - 227 °C430 - 440 °F
Die Temperature 221 - 229 °C430 - 445 °F
Melt Temperature 221 - 229 °C430 - 445 °FProcessing Temp
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
Swell1%;Aged 18 hrs at 121°C in Animal Fat. (ASTM D471)
 1%;Aged 18 hrs at 121°C in Vegetable oil. (ASTM D471)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation
DuPont Biomax® TPS 2501
Teknor Apex ELEXAR® EL 8730 Thermoplastic Elastomer
Teknor Apex Elexar® EL-8730A Thermoplastic Elastomer
Teknor Apex Terraloy™ MB 20001A Thermoplastic Starch + Copolyester

PTEKNO260 / 70003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.