117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity are required. It has outstanding heat resistance, excellent balance of high stiffness and toughness, and good contact clarity and gloss, low taste & odor transfer. It contains a nucleating agent and it Complies with U.S. FDA 21 CFR 177.1520. Information provided by Dow |