MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Zeniva® ZA-500 PEEK, Biomaterial
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Zeniva® ZA-500 is a grade of polyetheretherketone (PEEK) offered for use in implantable devices.

The manufacturing facility for Zeniva® PEEK in Alpharetta, GA is ISO 13485 registered and the relevant aspects of current Good Manufacturing Practices are also applied. The biomaterial manufacturing processes are carefully validated, and enhanced controls provide product traceability. In addition, all materials are tested in a lab that is ISO 17025 accredited. This product meets the requirements of the current version of ASTM F 2026.

Zeniva® ZA-500 is offered as resin pellets and fabricated forms such as rods and plates. The chemical, physical, and mechanical properties of finished parts are related to the processes utilized in producing the finished part (for example, molding, machining, annealing, sterilization, etc.).

An FDA MAF is available and a PMDA MF is available in Japan.

Applications: Body Implants; Medical/Healthcare Applications

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Viscosity 430 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
430 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 95.0 MPa13800 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Elongation at Yield 5.2 %5.2 %ASTM D638
Tensile Modulus 3.60 GPa522 ksiASTM D638
Flexural Yield Strength 150 MPa21800 psiASTM D790
Flexural Modulus 4.00 GPa580 ksiASTM D790
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 340 °C644 °FPeak; ASTM D3418
Crystallization Temperature 290 °C554 °FPeak; ASTM D3418
Glass Transition Temp, Tg 150 °C302 °FASTM E1356
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
Cytotoxicity - ISO 10993:5Pass
FormsPellets; Plate; Rod
Physiochemical Testing - ISO 10993:18Pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4636 / 280436

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.