MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF DTD Amine
Categories: Fluid

Material Notes: Formula: C26H55N

CAS: 900169-60-0

Description: Ditridecylamine mixture of isomers is a colorless to yellow liquid with an amine-like odor. It is not miscible with water.

Synonyms: 2-Imidazoleidinane, N,N’-Ethyleneurea, 2-Imidazolidone, 2-Oxoimidazolidin

Applications: Chemical intermediate, Floatation agents, Petroleum additives, Corrosion inhibitor, Plasticizers and Surfactants

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.836 g/cc0.0302 lb/in³
Molecular Weight 381.7 g/mol381.7 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -45.0 °C<= -49.0 °F
Boiling Point 220 - 240 °C428 - 464 °F
Flash Point 138 °C280 °F
Ignition Temperature 250 °C482 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %DIN 51 777
 
Descriptive Properties
Assay>90%
CompositionTridecane<0.5%
 Tridecanol<3.0%
 Tridecylamine<3.0%
 Tritridecylamine<10.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Evatane® 1350 VN 5 Ethylene Vinyl Acetate

PBASG0935 / 132568

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.