MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller Cyberbond ESH 22 Adhesive
Categories: Polymer; Adhesive

Material Notes: Profile: Sealant; low strength, high viscosity. Anaerobic adhesive: pipe- and flange sealant and instant gasket; easy to dismantle. Not classified as hazardous mixture. RoHS compliant.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/cc
Viscosity  7000 - 12000 cP
@Shear Rate 160 1/s
7000 - 12000 cP
@Shear Rate 160 1/s
cone-plate
 120000 - 250000 cP
@Shear Rate 0.500 1/s
120000 - 250000 cP
@Shear Rate 0.500 1/s
cone-plate
Storage Temperature 8.00 - 21.0 °C46.4 - 69.8 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 2.00 - 4.00 MPa290 - 580 psiCompressive
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.250 - 1.00 min0.00417 - 0.0167 hourSet time, M10 brass bolt/nut
 1440 min24.0 hourFull Cure
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive strength1-6 NmStainless steel V2A
 1-6 NmGalvanized steel
 2-6 NmSteel
 2-8 NmBrass
Base compoundDimethacrylate
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL035 / 316826

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.