MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering Z60B Hydrogenated NBR Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hydrogenated Nitrile Rubber, 55-65 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH614, A26, B36, EO16, EO36, F14.

Applications: High strength and excellent chemical resistance. Higher operating temperature than standard nitrile. Suitable for use with sour (H2S) crude oil and gas, which may also include lubricating, oil additives and amine corrosion inhibitors. Good resistance to weathering and ozone.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60°IRHD; ASTM D1415
 70°IRHD, +10 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 10.5 MPa-25% change after 70 hours @ 150°C; ASTM D412
 14.0 MPaASTM D412
Elongation at Break 175 %-30% change after 70 hours @ 150°C; ASTM D412
 250 %ASTM D412
Compression Set 50 %
@Temperature 150 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -20.0 °C
 -18.0 °CNon-brittle after 3 minutes
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Melos® FM 976 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Avient PolyOne® 4475 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Precision Polymer Engineering Z50B Hydrogenated NBR Compound
Avient PolyOne® ND-10 Ethylene-Propylene Diene Elastomer (EPDM) Compound
Avient PolyOne® 4763A Ethylene-Propylene Diene Elastomer (EPDM) Compound

PPRECI148 / 57872

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.