MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnol® H 5/50 A (LL 4311) Vinyl Chloride Copolymer
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: CAS NO. 25086-48-0

Product description: VINNOL® H 5/50 A (LL 4311) is a terpolymer of vinyl chloride (VC), vinyl acetate (VAc) and vinyl alcohol (VOH). Its main use is as a binder for surface coating compounds and printing inks.

Properties: VINNOL® H 5/50 A (LL 4311) is a thermoplastic, physically drying, binder that forms a film when the solvent contained in the formulation has evaporated. Like all VC copolymers, VINNOL® H 5/50 A (LL 4311) is characterized by excellent toughness, permanent flexibility, abrasion resistance, low swelling in the presence of water, and low gas permeability. Films of VINNOL® H 5/50 A (LL 4311) are highly resistant to water. They also show excellent resistance to oil, grease, diluted aqueous acids, alkaline and saline solutions. VINNOL® H 5/50 A (LL 4311) is resistant to aliphatic hydrocarbons, such as white spirit, and to alcohols.

Special features: VINNOL® H 5/50 A (LL 4311) contains approx. 2% free hydroxyl groups and can therefore also be used in reactive coating and ink systems. For example it may be crosslinked with isocyanates, epoxy or melamine resins.

Application: Typical applications for VINNOL® H 5/50 A (LL 4311):

  • Primers
  • Printing inks
  • Intermediate coatings
  • Two-pack coating systems
  • Baking finishes
  • Adhesives

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 g/cc0.0271 lb/in³DIN EN ISO 60
Density 1.39 g/cc0.0502 lb/in³DIN 66137-2
Volatiles <= 1.0 %<= 1.0 %
Particle Size <= 1000 µm<= 1000 µm
Viscosity 80 - 120 cP80 - 120 cP20% solids in MEK; DIN 53015
Molecular Weight 60000 - 80000 g/mol60000 - 80000 g/mol
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 74.0 °C165 °FDIN 53765/ISO 11357-5
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 50 - 53 %50 - 53 %
 
Descriptive Properties
K-Value50-52DIN EN ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9675 / 205204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.