MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 8617H Steel, heat treated, machined, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Normalized 925°C (1700°F) in 32 mm rounds, machined to 25 or 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8 hours, box cooled to room temperature, reheated to 800°C (1470°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds. Post oil quenched hardness 25 mm: 302 HB at 7/8 radius, 265 HB at half-radius, 258 HB at center; 50 mm: 235 HB at 7/8 radius, 215 HB at half-radius, 207 HB at center

Key Words: AFNOR 22 NCD 2 (Fr), UNI 10 NiCrMo, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20, 805 M 20, UNS H86170, ASTM A304, SAE J1268, DIN 1.6523, AFNOR 20 NCD 2 (Fr)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 233233
Hardness, Knoop 257257Converted from Brinell
Hardness, Rockwell B 9696Converted from Brinell
Hardness, Rockwell C 2020Converted from Brinell
Hardness, Vickers 245245Converted from Brinell
Tensile Strength, Ultimate 786 MPa114000 psi
Tensile Strength, Yield 530 MPa76900 psi
Elongation at Break 22 %22 %in 50 mm
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steels
Poissons Ratio 0.290.29Calculated
Machinability 70 %70 %hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000234 ohm-cm0.0000234 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FTypical steel
Thermal Conductivity 46.6 W/m-K323 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.14 - 0.20 %0.14 - 0.20 %
Chromium, Cr 0.35 - 0.65 %0.35 - 0.65 %
Iron, Fe 96.825 - 98.21 %96.825 - 98.21 %As remainder
Manganese, Mn 0.65 - 0.95 %0.65 - 0.95 %
Molybdenum, Mo 0.15 - 0.25 %0.15 - 0.25 %
Nickel, Ni 0.35 - 0.75 %0.35 - 0.75 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 8617 Steel, heat treated, machined, pseudocarburized, reheated to 855°C (1570°F), 150°C (300°F) temper
AISI 8617H Steel, heat treated, machined, pseudocarburized, reheated to 855°C (1570°F), 150°C (300°F) temper
AISI 8617 Steel, heat treated, machined, pseudocarburized, 150°C (300°F) temper
AISI 8617H Steel, heat treated, machined, pseudocarburized, 150°C (300°F) temper
AISI 8617 Steel, heat treated, machined, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper

M861CC / 8279

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.