MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phosphorus-Deoxidized, High Residual Phosphorus, UNS C12200, M20 Temper, Flat
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Hot Rolled

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Butt Weld

Common Fabrication Processes: Blanking, Coining, Coppersmithing, Drawing, Etching, Forming and Bending, Heading and Upsetting, Hot Forging and Pressing, Piercing and Punching, Roll Threading and Knurling, Shearing, Spinning, Squeezing and Swaging, Stamping

Typical uses: Downspouts; Flashing; Gutters; Roofing; Air Lines; Hydraulic Lines; Oil Lines; Air Conditioner Tubes and Condenser Sheets; Gas Lines; Heater Lines; Oil Burner Tubes; Air Conditioners; Refrigerators; Heater Elements; Wire Connectors; Air Lines in Airplanes; Anodes for Electroplating; Brewery Tubes; Casting Molds; Condenser Tubes; Dairy Tubes; Distiller Tubes; Evaporator Tubes; Expansion Joint Tubes; Gage Lines; Gasoline Lines in Airplanes; Heat Exchanger Shells; Hydraulic Lines in Airplanes; Kettles; Oil Coolers in Airplanes; Oil Lines in Airplanes; Paper Lines; Plating Anodes; Plating Hangers; Plating Racks; Plumbing Tube; Print Rolls; Rotating Bands; Steam Lines; Sugar House Refinery Lines; Tanks; Tubing, LP Gas Service; Tubing, Medical Gas- Oxygen; Water Lines; Gasoline Lines; Oil Coolers; Plumbing Fittings; Plumbing Pipe

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F  40
@Thickness 6.35 mm
40
@Thickness 0.250 in
 45
@Thickness 1.02 mm
45
@Thickness 0.0400 in
Tensile Strength  165 MPa
@Thickness 1.02 mm
24000 psi
@Thickness 0.0400 in
 221 MPa
@Thickness 6.35 mm
32000 psi
@Thickness 0.250 in
Tensile Strength, Yield  68.9 MPa
@Thickness 6.35 mm
10000 psi
@Thickness 0.250 in
0.5% Ext
 68.9 MPa
@Thickness 1.02 mm
10000 psi
@Thickness 0.0400 in
0.5% Ext
Elongation at Break  45 %
@Thickness 1.02 mm
45 %
@Thickness 0.0400 in
 50 %
@Thickness 6.35 mm
50 %
@Thickness 0.250 in
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
Forgeability 65 %65 %
Shear Strength  152 MPa
@Thickness 6.35 mm
22000 psi
@Thickness 0.250 in
 159 MPa
@Thickness 1.02 mm
23000 psi
@Thickness 0.0400 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 ohm-cm0.00000200 ohm-cm85% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.40 µin/in-°F
@Temperature 68.0 - 212 °F
 17.1 µm/m-°C
@Temperature 20.0 - 200 °C
9.50 µin/in-°F
@Temperature 68.0 - 392 °F
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 28.2 W/m-K196 BTU-in/hr-ft²-°F
Melting Point <= 1083 °C<= 1981 °F
Liquidus 1083 °C1981 °F
Annealing Point 399 - 649 °C750 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature >= 760 °C>= 1400 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.9 %>= 99.9 %
Phosphorus, P 0.015 - 0.040 %0.015 - 0.040 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC12200x4 / 292742

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.