MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lotte Advanced Materials MPEG-1200 Methoxy Polyethylene Glycol Monomer
Categories: Other Engineering Material

Material Notes: Narrow molecular distribution; Low Free-PEG content (under 2 wt%); Low Dioxane and Free-EO content

Applications: Polycarboxylate superplasticizer; Methyl-blocked fatty acid PEG esters, raw material of concrete admixtures

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 5.50 - 7.505.50 - 7.50ISO 4316
Molecular Weight 1100 - 1300 g/mol1100 - 1300 g/mol
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.100 %<= 0.100 %ASTM D1744
 
Descriptive Properties
AppearancePaste
Color<100 APHA50?, ASTM D1209
Content<5 ppmDioxane
 <5 ppmFree EO
 43-51 /gHydroxyl Value, ASTM D4252

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9381 / 325863

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.