MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 9832 Double Coated Tapes with Adhesive 300MP
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape is well suited for applications requiring temperature performance up to 250°F for short term exposure and up to 150°F for long term exposure. A thin polyester film carrier provides dimensional stability and improved handling.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.7 microns0.500 milCarrier
 50.8 microns2.00 milBackside Adhesive
 58.4 microns2.30 milFaceside Adhesive
 102 microns4.00 milLiner Caliper
 122 microns4.80 milTotal Thickness
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.3725 kN/m2.125 pliPolypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.614 kN/m3.50 pliStainless Steel, 90°, 15 min RT; ASTM D3330
 0.6355 kN/m3.625 pliStainless Steel, 90°, 72 hr RT; ASTM D3330
 0.6355 kN/m3.625 pliABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.7231 kN/m4.125 pliPolycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.9422 kN/m5.375 pliStainless Steel, 90°, 72 hr 158°F; ASTM D3330
 1.030 kN/m5.875 pliStainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.6 °C150 °FLong Term
 121 °C250 °FShort Term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
LinerTan, 58# Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33302 / 168049

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.