MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels
Categories: Ceramic

Material Notes: Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives.

Applications

  • Pot cradle insulation (for Alcoa A-697 pots)
  • Precipitators
  • Dryers
  • Ducts and breeching
  • Utility boilers
  • Furnaces
  • Kilns

Advantages

  • Excellent mechanical strength in non-fired condition
  • Refractory ceramic fiber free
  • Low thermal conductivity
  • Use of large-size boards to reduce labor costs
  • Material can be cut quickly by hand with knife or saw for fabrication and application on the job

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.296 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000660 GPa
Compressive Strength 0.230 MPanon-fired at 10% compressions
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0700 W/m-K
@Temperature 260 °C
 0.0900 W/m-K
@Temperature 371 °C
 0.120 W/m-K
@Temperature 482 °C
Maximum Service Temperature, Air 1038 °C
Shrinkage <= 2.5 %
@Temperature 1038 °C,
Time 86400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast XL Small Component Refractory
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Pyrocast TG Castable Refractory
Pyrotek Pyromat TS-045 Electrical Insulating Board
Pyrotek Pyrocast ZS Refractory Shapes

CPYRO204 / 1921

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.