MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI 1010 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round or thickness
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Easily cold formed by heading, extruding, upsetting, bending, and other deforming processes. Uses for wires include electroplated products, such as racks, storage bins, shopping carts, fan guards, and jewelry, and unplated such as wires, staples, hardware, and barbed wire.

Key Words: UNS G10100, AMS 5040, AMS 5042, AMS 5044, AMS 5047, AMS 5053, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A545, ASTM A549, ASTM A575, ASTM A576, MIL SPEC MIL-S-11310 (CS1010), JIS S 9 CK, SAE J403, SAE J412, SAE J414, DIN 1.1121, AFNOR XC 10 (Fr), JIS S10 C, JIS S 12 C, AISI1010
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccTypical for steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 105
Hardness, Knoop 123Converted from Brinell
Hardness, Rockwell B 60Converted from Brinell
Hardness, Vickers 108Converted from Brinell
Tensile Strength, Ultimate 365 MPa
Tensile Strength, Yield 305 MPa
Elongation at Break 20 %in 50 mm
Reduction of Area 40 %
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical For Steel
Machinability 55 %Based on AISI 1212 steel = 100%. Group I bar, rod, and wire products machinability can be improved by cold drawing.
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000143 ohm-cmcondition unknown
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.2 µm/m-°C
@Temperature 0.000 - 100 °C
 13.0 µm/m-°C
@Temperature 0.000 - 200 °C
 13.5 µm/m-°C
@Temperature 0.000 - 300 °C
 13.8 µm/m-°C
@Temperature 0.000 - 400 °C
 14.2 µm/m-°C
@Temperature 0.000 - 500 °C
 14.6 µm/m-°C
@Temperature 0.000 - 600 °C
 14.9 µm/m-°C
@Temperature 0.000 - 700 °C
Specific Heat Capacity 0.448 J/g-°C
@Temperature >=100 °C
condition unknown
 0.498 J/g-°C
@Temperature 150 - 200 °C
 0.519 J/g-°C
@Temperature 200 - 250 °C
 0.536 J/g-°C
@Temperature 250 - 300 °C
 0.565 J/g-°C
@Temperature 300 - 350 °C
 0.590 J/g-°C
@Temperature 350 - 400 °C
 0.649 J/g-°C
@Temperature 400 - 450 °C
 0.729 J/g-°C
@Temperature 550 - 600 °C
 0.825 J/g-°C
@Temperature 650 - 700 °C
Thermal Conductivity 51.9 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.080 - 0.13 %
Iron, Fe 99.18 - 99.62 %As remainder
Manganese, Mn 0.30 - 0.60 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
AISI 1010 Steel, cold drawn
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
AISI 1008 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round

M1010C / 6784

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.