MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® LDPE Powder 2102P5 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE Powder 2102P5 is an additive free standard CTR® tubular grade for masterbatch with a relatively low melt flow rate. This grade is supplied in powder form. Application SABIC® LDPE Powder 2102P5 is a general medium sized powder grade, typical used for textile coating, carpet backing and compounding applications with a low viscosity. Further it can be used for low filled or additive masterbatches (e.g. slip agents, anti fog agents, anti static agents, thermal stabilizers). This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.340 g/cc0.0123 lb/in³ASTM D1895
Density 0.921 g/cc0.0333 lb/in³ASTM D1505
Particle Size <= 600 µm<= 600 µmASTM D1921
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 110 J/g47.3 BTU/lbSABIC method
Melting Point 109 °C228 °FSABIC method
Vicat Softening Point 91.0 °C196 °Fat 10 N (VST/A); ISO 306
 
Descriptive Properties
Dry flow23 secISO 6186

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11028 / 244495

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.