A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is normally used in the printed circuit board industry as a backup for the drilling operation. However, it is also used in other industries for tooling stock because of its ease of machining and good dimensional stability.Information provided by Norplex-Micarta |
Paper, Phenolic, backer board, Micarta |