MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

ALM PA-616-GS Filled Nylon 12 Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:
  • 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.
  • The PA 616-GS can be processed on any laser sintering platform, but has been specifically engineered for EOS platforms.
  • PA 616-GS is slightly less recyclable when compared to PA 615-GS, but produces a smooth part surface finish.

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 g/cc0.0271 lb/in³ASTM D1895
Density 1.49 g/cc0.0538 lb/in³ASTM D792
Particle Size 50 µm50 µmD50
 35 - 100 µm35 - 100 µmD10-D90
Melt Flow 35 - 45 g/10 min
@Load 5.00 kg,
Temperature 235 °C
35 - 45 g/10 min
@Load 11.0 lb,
Temperature 455 °F
3 min; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 31.0 MPa4500 psiXY; ASTM D638
Elongation at Break 1.4 %1.4 %XY; ASTM D638
Tensile Modulus 4.10 GPa595 ksiXY; ASTM D638
Flexural Modulus 3.10 GPa450 ksiXY; ASTM D790
Izod Impact, Notched 0.960 J/cm1.80 ft-lb/inASTM D256
Izod Impact, Unnotched 1.01 J/cm1.89 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm50% RH, 500V; ASTM D257
Surface Resistance 2.30e+14 ohm2.30e+14 ohm50% RH, 500V; ASTM D257
Dielectric Constant 3.73.7ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 186 °C367 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin
EMS-Grivory Grilamid® TR 90 UV PAMACM12
EMS-Grivory Grilamid® TR 90 TL PAMACM12
EMS-Grivory Grilamid® TR 90 PAMACM12
EMS-Grivory Grilamid® TR 55 PA12/MACMI

PALP86 / 177147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.