Hostacom FPP 20/10 TGF BLK is a 10% talc filled and 10% glass fiber reinforced PP homopolymer with high strength and low warpage. Availability: Europe Application: White Goods Market: Electrical / Electronics Processing Method: Injection Molding Information provided by LyondellBasell. |