Temperature range: 1350-1650°C. Manufacturing method: cast. The IFB range is manufactured via cast (K®) and slinger (JM™) processes, is a market leader in applications such as Petrochemical and Ceramics where the ability to operate in environments above 1000°C (1800°F) is critical. The range also provides low thermal conductivity due its unique manufacturing process. Our IFBs deliver energy savings for multiple markets and our global manufacturing footprint enables Morgan to meet your regional and global application demands. Applications: Hot face refractory lining or as back-up insulation in: - Aluminium (anode bake furnaces, primary electrolytic cells, holding and melting furnaces and secondary re-melt furnaces)
- Petrochemical (kilns, flues, refining vessels and heaters and reactor chambers)
- Iron and steel industry (heat treatment and galvanising)
- Coke and iron making (blast furnaces, hot blast stoves, hot blast and bustle main)
- Hobby and laboratory kilns
- Ceramic industry (including kilns for domestic use)
- Lime and cement kilns
- Glass industry
Information provided by Morgan Advanced Materials |