MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ B-46 Adhesive, Sealant & Coating System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties: Excellent adhesion to low surface energy plastics without primer or surface preparation.

Applications: Very high flexibility, 500% elongation, emphasizing high tack for un-abraded substrates and plastic films, including unetched Teflon. Excellent water and oil block for cable application. Ambient or thermal cure.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 1.0 %
Viscosity 1500 cP
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -50.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 480 minAmbient Set
 4320 minAmbient, 95% cure
 240 min
@Temperature 93.3 °C
98% cure
Tack-Free Time 1440 minAmbient
Pot Life 90 minAmbient
 
Descriptive Properties
Chemical & Moisture Resistance10=Lowest, 4=Highest
ColorClear with haze/slight amber
Flexibility Ranking50=Rigid, 5=Highly Flexible

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Unreinforced
Aluminum 390.0-T6 Acurad Castings
Aluminum 6061-T6; 6061-T651
Overview of materials for Epoxy Cure Resin
Aluminum A390.0-T6, Permanent Mold Cast

PAQREL03 / 24219

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.