MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson IPP Rubber Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: N-isopropyl-N’-phenyl-p-phenylene

Molecular Formula: C15H18N2

CAS#: 101-72-4

Properties: soluble in gasoline, benzene, acetone and etc. Insoluble in water.

Applications: It is an antioxidant used for rubber products with high efficiency, low poison and low solvent-extraction amount. Also used as stabilizer in synthetic rubber. It’s main used in tire, rubber shoes, belt, hoses automotive mounts so on. IPPD is regulated for use in articles in contact with food as specified under FDA 21 CFR 177.2600 and under BGVV XXI, Categories 3-4.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 227 g/mol227 g/mol
Ash <= 0.20 %<= 0.20 %
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 70.0 °C>= 158 °FInitial
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AppearanceGray purple to dark purple brown pastilles
Assay>96%
Heat Loss<0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS050 / 256095

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.