MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Palm Labs Adhesives TURBO-LOCK SERIES 20 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO-LOCK SERIES 20 is a fast curing, BLUE, low strength, thread locker for bonding and sealing small plastic fasteners. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals.

Application: Will join fitted cylindrical small plastic screws and bolts.

Part Numbers for this data: 20-001, 20-028, 20-056, 20-454

Solubility: Turbo Debonder

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 9011-14-7 and 123-31-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 80 cP80 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 6565
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.33
@Frequency 1e+6 Hz
3.33
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point 82.2 °C180 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.50 min0.0250 hourHandling
 3.00 min0.0500 hourFunctional
 1440 min24.0 hourFull
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlue
CompositionEthyl Cyanoacrylate
Gap Fill1/4"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALML050 / 135204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.