MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kazanorgsintez Ethyleneglycol
Categories: Fluid; Solvent

Material Notes: Production Method: Obtained by hydration of ethylene oxide.

Application: Intended for use in the production of synthetic fibers, resins, solvents, low-freezing and hydraulic fluids, and for other purposes.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.43 - 1.4321.43 - 1.432First Class
 1.431 - 1.4321.431 - 1.432Premium Quality
UV Transmittance  >= 75 %
@Wavelength 220 nm
>= 75 %
@Wavelength 220 nm
Premium Quality
 >= 95 %
@Wavelength 275 nm
>= 95 %
@Wavelength 275 nm
Premium Quality
 >= 100 %
@Wavelength 350 nm
>= 100 %
@Wavelength 350 nm
Premium Quality
 
Descriptive Properties
Color20Hazen units, in an ordinary state, First Class
 20Hazen units, after boiling with hydrochloric acid, Premium Quality
 5Hazen units, in an ordinary state, Premium Quality
Mass Content (%)0.0006Mass content of acids in conversion to acetic acid, Premium Quality
 0.001Mass content of residue after calcination, Premium Quality
 0.002Mass content of residue after calcination, First Class
 0.005Mass content of acids in conversion to acetic acid, First Class
 0.05Mass content of diethylene glycol, Premium Quality
 1Mass content of diethylene glycol, First Class
 98.5Mass content of ethylene glycol, First Class
 99.8Mass content of ethylene glycol, Premium Quality

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN140 / 127459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.