MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Momentive Performance Materials TSE 326M EX Heat Curable Silicone Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: TSE326M EX is a one-component, heat curable silicone adhesive designed for high temperature applications. TSE326M EX adheres well to a variety of substrates, such as metals, plastics, ceramics and glass without the use of a primer.

Features: Ready to use – one component, Excellent high temperature resistance, Heat accelerated cure, Excellent adhesive properties; Primerless adhesion to many types of substrates, Non corrosive to metals.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³Cured
Viscosity 16000 cP16000 cPUncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838
Tensile Strength 2.90 MPa421 psi
Elongation at Break 180 %180 %
Adhesive Bond Strength 1.50 MPa218 psiAluminum lap shear.
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmCured
Dielectric Constant 3.3
@Frequency 60 Hz
3.3
@Frequency 60 Hz
Cured
Dielectric Strength 22.0 kV/mm559 kV/inCured
Dissipation Factor 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
Cured
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°FCured
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 200 °C
0.500 hour
@Temperature 392 °F
as tested
 90.0 min
@Temperature 150 °C
1.50 hour
@Temperature 302 °F
 180 min
@Temperature 120 °C
3.00 hour
@Temperature 248 °F
 
Descriptive Properties
AppearanceFlowableUncured
ColorReddish brownCured
 Reddish brownUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9901 / 265710

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.