MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 GLW-E ISO 320
Categories: Fluid; Lubricant

Material Notes: AGMA Grade 6 EP

GLW is a premium quality, extreme-pressure (EP) industrial gear oil developed for the lubrication of heavily loaded enclosed gear drives operating under severe service conditions. It is specially formulated to quickly separate from water to maintain effective lubrication in the presence of water. It is particularly recommended for use in industrial and mining equipment operating in contaminated environments where an AGMA EP gear oil with excellent water-separating properties is specified or preferred. GLW is formulated to provide excellent lubricity and wear protection even in the presence of water and other contaminants. It has high load-carrying capacity, high film strength, and protects against rust and corrosion for extended equipment life. It has good oxidation resistance and thermal stability at high temperatures and is formulated with “clean gear” additive technology to minimize deposit formation and provide outstanding gearbox cleanliness. It has good seal compatibility, excellent water-separating properties and is resistant to excessive foam buildup that can interfere with proper lubrication. GLW is recommended for use in Joy Machinery longwall mining equipment as well as other mining, industrial and heavy mobile equipment operating under extreme loads and/or exposed to water contamination.

Applications:

  • Enclosed gear drives of longwall mining machinery
  • Enclosed industrial gear drives operating in the presence of water, such as in steel mills and rock quarries
  • Gear drives and pinion stands of metal rolling mills, ball mills and cement mills
  • Enclosed gear drives on excavation and heavy construction equipment
GLW meets the requirements of the following industry and OEM specifications:
  • ANSI/AGMA Standard 9005-E02, Anti-Scuff/Anti-Wear (EP) Oils
  • DIN 51517 Part 3, Lubricating Oils, Type CLP
  • German Steel Industry SEB 181226, Type CLP
  • ISO 12925-1, Type L-CKC & Type L-CKD
  • Joy Mining Machinery TO-MEP (ISO VG 220), TO-HEP(ISO VG 320), TO-HD(ISO VG 460)
  • U.S. Steel 224
Features/Benefits:
  • Excellent performance in wet or contaminated gearboxes
  • Outstanding load-carrying capacity
  • Excellent protection against scuffing and wear
  • Good oxidation resistance and thermal stability
  • Outstanding deposit control for gearbox cleanliness
  • Protects against rust and corrosion
  • Emulsifies readily with water
  • Good seal compatibility
  • Environmentally responsible; does not contain chlorinated paraffin

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.893 g/cc
Density 7.44 lb/gal
Viscosity Measurement 93Index
Saybolt Viscosity at 100°F 1723 SUS
Saybolt Viscosity at 210°F 118 SUS
Kinematic Viscosity at 40°C (104°F) 323 cSt
Kinematic Viscosity at 100°C (212°F) 23.7 cSt
ASTM Color 5.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 1.09[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 57[kg]; ASTM D2596
Four Ball Extreme Pressure, Weld Load 315 kgASTM D2596
Four Ball Wear 0.260 mmScar Diameter; ASTM D4172
Timken Test 70.0 lbOK Load; ASTM D2782
 
Thermal PropertiesOriginal ValueComments
Pour Point -18.0 °C
Flash Point 254 °CCOC
 
Descriptive Properties
Copper Corrosion1bASTM D130
FZG Scuffing Test>14 Failure Load StageASTM D5182
Oxidation Stability0.055Viscosity Increase @ 121°C, ASTM D2893

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5101 / 198354

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.