MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

SABIC LNP™ LUBRICOMP™ KP003AXZ Acetal Homopoly (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ASTM D 792
 1.47 g/cc0.0531 lb/in³ISO 1183
Moisture Absorption 0.300 %
@Time 86400 sec
0.300 %
@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow  0.024 cm/cm
@Time 86400 sec
0.024 in/in
@Time 24.0 hour
ASTM D 955
 0.024 cm/cm
@Time 86400 sec
0.024 in/in
@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse  0.025 cm/cm
@Time 86400 sec
0.025 in/in
@Time 24.0 hour
ASTM D 955
 0.025 cm/cm
@Time 86400 sec
0.025 in/in
@Time 24.0 hour
ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.0 MPa7540 psiASTM D 638
 53.0 MPa7690 psiISO 527
Tensile Strength, Yield 53.0 MPa7690 psiASTM D 638
 53.0 MPa7690 psiISO 527
Elongation at Break 15.1 %15.1 %ISO 527
 28.8 %28.8 %ASTM D 638
Elongation at Yield 15 %15 %ISO 527
 20.9 %20.9 %ASTM D 638
Tensile Modulus 2.57 GPa373 ksi1 mm/min; ISO 527
 2.75 GPa399 ksi50 mm/min; ASTM D 638
Flexural Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 2.75 GPa399 ksiASTM D 790
 3.00 GPa435 ksiISO 178
Izod Impact, Notched 0.530 J/cm
@Temperature 23.0 °C
0.993 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 10.14 J/cm
@Temperature 23.0 °C
19.00 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 53.0 kJ/m²
@Temperature 23.0 °C
25.2 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
Instrumented Impact Energy at Peak 1.00 J
@Temperature 23.0 °C
0.738 ft-lb
@Temperature 73.4 °F
ASTM D 3763
Coefficient of Friction, Dynamic 0.210.21ASTM D 3702 Modified: Manual
Coefficient of Friction, Static 0.110.11ASTM D 3702 Modified: Manual
K Factor (Wear Factor) 111110^-10 in^5-min/ft-lb-hr; Washer; ASTM D 3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  95.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
 96.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  95.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
 96.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 157 °C315 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 162 °C
@Thickness 3.20 mm
324 °F
@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 92.0 °C
@Thickness 3.20 mm
198 °F
@Thickness 0.126 in
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® L 20 L PA12

PSABI48002 / 189087

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.