MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® DigiPrime® 4450 Primer
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Print receptive primer for HP Indigo ElectroInks®.

Usage: DigiPrime® 4450 is a ready to use primer which provides excellent adhesion of HP Indigo ElectroInks® to a wide variety of films and papers. This product has exceptional anti-block properties and can be used for two sided printing. It also has food contact approval.

Application data: DigiPrime® 4450 may be applied by flexo, gravure, rod or roll coating system. Recommended application rate for films is between 0.5 to 0.2 gsm dry coat weight. For paper slightly higher weights will be needed to overcome the absorption of the substrate, this will vary from paper to paper but dry weights around 0.7 to 1 gsm are recommended.

When manufactured in Belgium and the USA product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1(Restricted) and Commission Regulation (EU) n° 10/2011(Restricted)
Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)

Food Contact Information when manufactured in USA:
FDA:
175.105: Components of adhesives
175.300: Resinous and polymeric components of coatings(Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Food Contact Information when manufactured in Belgium:
FDA:
175.105: Components of adhesives
175.300: Resinous and polymeric components of coatings(Restricted).
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.02 g/cc1.00 - 1.02 g/cc
Volatiles 68 - 70 %68 - 70 %
pH 8.0 - 108.0 - 10
Brookfield Viscosity <= 100 cP<= 100 cPSpindle # 1, rpm 60
 
Descriptive Properties
AppearanceWhite, translucent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets

WMICHEL014 / 134931

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.