MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo TYRIL™ 867 E UV Styrene-Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: TYRIL™ styrene-acrylonitrile (SAN) resins are designed to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications. The key property of TYRIL 867 E is excellent balance of physical properties. TYRIL 867 E is specifically designed to provide good processability, good chemical and heat resistance and very good strength. The UV-stabilized version exhibits excellent weatherability, suitable in particular for extruded sheet and thermoforming applications.

Applications:

  • Extruded sheet for shower cabinets, or glazing
  • Sanitary accessories: soap dishes, toilet seats

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Apparent Bulk Density 0.690 g/cc0.0249 lb/in³ISO 60
Melt Flow  4.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
12 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8383ASTM D785
Tensile Strength at Break 70.0 MPa10200 psi5 mm/min; ASTM D638
 70.0 MPa10200 psiISO 527-2/5
Tensile Modulus 3.70 GPa537 ksiISO 527-2/5
Flexural Strength 97.0 MPa14100 psiASTM D790
Izod Impact, Unnotched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 9.10 kV/mm231 kV/inIEC 60243-1
Dissipation Factor 0.00010
@Frequency 1e+6 Hz
0.00010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C27.8 µin/in-°FDIN 53752
Specific Heat Capacity 1.38 J/g-°C0.330 BTU/lb-°FASTM D2766
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FAnnealed; ISO 75-2/A
Vicat Softening Point 101 °C214 °FISO 306/B50
 110 °C230 °FISO 306/A120
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dyna-Purge® C Purging Compound
RTP Company RTP 501 UV  Styrene Acrylonitrile (SAN) Glass Fiber 10% - UV Stable
Network Polymers SAN 300 Natural
Network Polymers SAN 280 Water Clear

PTRINS9099 / 197572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.