MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot BLACK PEARLS® 900 Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: BLACK PEARLS 900 specialty carbon black offers the highest level of jetness available within Cabot’s specialty carbon black portfolio for plastics applications. It can enable masterbatch and compound producers to meet increasingly stringent requirements for deep black color in visible molded parts in automotive and electronics applications.

Key applications: BLACK PEARLS 900 specialty carbon black can deliver high jetness in conjunction with good blue undertone. As a result, it is often used in highly demanding applications where OEMs require very deep black color in plastic molded parts. Applications are primarily:

  • Consumer electronics
  • Automotive interiors
  • Home appliances
BLACK PEARLS 900 specialty carbon black is typically used in ABS, PC blends, PP, and TPOs for aesthetic applications. Because of its dispersion characteristics, it is typically incorporated into a compound via masterbatch. To achieve optimal performance levels with this product, incorporation into a masterbatch requires relatively sophisticated, high shear processing conditions. BLACK PEARLS 900 specialty carbon black is a pelletized product. A non-pelletized carbon black having similar morphology is available in an easier-to-disperse fluffy form as MONARCH 900 specialty carbon black, which can also be used in coatings and artificial leather applications.

Performance features:

  • Highest level of jetness performance within Cabot’s portfolio of carbon blacks for plastic applications
  • Good blue undertone performance

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.440 g/ccASTM D-1513
Particle Mesh Size 325 Mesh<100 ppm; ASTM D-1514
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 3.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption258 mg/gASTM D-1510
OAN64 cc/100gASTM D-2414
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT037 / 315772

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.