MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cast Stainless Steel CG8M, ASTM A744
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes: Corrosion resistant, severe service

Key Words: ASTM A744/A744M(98)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 520 MPa>= 75400 psi
Tensile Strength, Yield >= 240 MPa>= 34800 psi
Elongation at Break >= 25 %>= 25 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 21 %18 - 21 %
Iron, Fe 58.8 - 70 %58.8 - 70 %As remainder
Manganese, Mn <= 1.5 %<= 1.5 %
Molybdenum, Mo 3.0 - 4.0 %3.0 - 4.0 %
Nickel, Ni 9.0 - 13 %9.0 - 13 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.5 %<= 1.5 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Stainless Steel CN7MS, ASTM A744
Cast Stainless Steel CG8M, ASTM A743
MetalTek MTEK 317 Cast UNS J93000 Austenitic Stainless Steel
Cast Stainless Steel CG8M, UNS J93000
AISI Type 304L Stainless Steel

MQCCG8MA40 / 13396

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.