The characteristics of Sandvik 20C strip steel are:Excellent surface finishGood flatnessGood etchabilityHigh strength and wear resistance Low level of non-metallic inclusionsGood dimensional tolerances Information provided by Sandvik ASTM 1095; EN 1.1274 |