MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® RG-20170 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-20100 series is group of high performance thermoplastic elastomer specifically designed for extruded regulated applications including food contact, toys and children’s products. Monprene RG-20170 is a low density, Medium hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: BPA Free, Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Low Flow; Low Density; Low Specific Gravity; Lubricated; Medium Hardness; No Animal Derived Components; Slip; Without Fillers

Uses: Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  70
@Time 5.00 sec
70
@Time 0.00139 hour
Injection Molded; ISO 868
 73
@Time 1.00 sec
73
@Time 0.000278 hour
Injection Molded; ISO 868
Tensile Strength at Break 6.20 MPa899 psi20 in/min, Flow; ASTM D412
 10.5 MPa1530 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  2.88 MPa
@Strain 100 %
417 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 3.85 MPa
@Strain 300 %
559 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 4.96 MPa
@Strain 100 %
720 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 5.68 MPa
@Strain 300 %
824 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 180 %180 %20 in/min, Flow; ASTM D412
 780 %780 %20 in/min, Across Flow; ASTM D412
Tear Strength 31.6 kN/m180 pliMethod Ba, Angle (Unnicked), 20 in/min, Across Flow; ISO 34-1
 33.3 kN/m190 pliMethod Ba, Angle (Unnicked), 20 in/min, Flow; ISO 34-1
Compression Set  27 %
@Temperature 22.8 °C,
Time 79200 sec
27 %
@Temperature 73.0 °F,
Time 22.0 hour
Type A; ISO 815
 44 %
@Temperature 70.0 °C,
Time 79200 sec
44 %
@Temperature 158 °F,
Time 22.0 hour
Type A; ISO 815
 
Processing PropertiesMetricEnglishComments
Zone 1 149 - 160 °C300 - 320 °F
Zone 2 160 - 204 °C320 - 400 °F
Zone 3 171 - 216 °C340 - 420 °F
Zone 4 182 - 227 °C360 - 440 °F
Die Temperature 182 - 227 °C360 - 440 °F
 
Descriptive Properties
AppearanceColors Available
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0943 / 237434

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.