MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.

Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Screen Pack: 60/60 Screw: 3:1 to 3.5:1 compression ratio screw PVC screw

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccASTM D792
Viscosity 35000 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
 1.20e+6 cP
@Shear Rate 67 1/s,
Temperature 200 °C
ASTM D3835
Maximum Moisture Content 0.020
Deformation 40 %
@Temperature 150 °C
300g; UL 1581
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9210 sec; ASTM D2240
Tensile Strength at Break 24.1 MPaUL 1581
 17.9 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 240 %UL 1581
 240 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.42
@Frequency 50 Hz
IEC 60250-1969; IEC 60250
Dielectric Strength 51.0 kV/mmIEC 60243-1
Dissipation Factor 0.0060
@Frequency 50 Hz
IEC 60250-1969
 
Processing PropertiesOriginal ValueComments
Zone 1 180 - 190 °C
Zone 2 185 - 200 °C
Zone 3 185 - 210 °C
Zone 4 185 - 210 °C
Die Temperature 195 - 220 °C
Drying Temperature 70.0 - 81.1 °C
Dry Time 4.00 - 8.00 hour
 
Descriptive Properties
AppearanceNatural Color
FeaturesFlame Retardant
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesWire & Cable Applications
VW-1passUL 1581

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE)
Teknor Apex Laripur® LPR 9060EF Thermoplastic Polyurethane
Avient OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)

PH0POL1415 / 145984

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.