MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alfa Chemistry Materials Zinc stearate
Material Notes: Applications: It is widely used as a release agent for the production of many kinds of objects rubber, poly urethane, polyester processing system, powder metallurgy. These applications exploit its "non-stick" properties . In cosmetics, zinc stearate is a lubricant and thickening to improve texture. It is an "activator" for rubber vulcanization by sulfur and accelerators. As discovered in the early days of vulcanization, zinc has a beneficial effect on the reaction of the sulfur with the polyolefin. The stearate is a form of zinc that is highly soluble in the nonpolar medium of the poly olefins. Being lipophilic, it functions as a phase transfer catalyst for the saponification of fats. Zinc stearate is used in cosmetic formulations to increase adhesive properties. It is also used as a coloring agent. This is a mixture of the zinc salts of stearic and palmitic acids. Zinc stearate is primarily used in pharmaceutical formulations as a lubricant in tablet and capsule manufacture at concentrations up to 1.5% w/w. It has also been used as a thickening and opacifying agent in cosmetic and pharmaceutical creams, and as a dusting powder.

ZINC STEARATE is a white, hydrophobic powder with a slight, characteristic odor. Insoluble in water, ethyl alcohol and diethyl ether. Soluble in acids. Non-toxic. In technical grades, the percentage of zinc may vary according to the intended use. Products with less than the theoretical amount of zinc are more acidic.

Synonyms: Zinc distearate; Zn Stearate; Zincum stearinicum; Zink distearat; Octadecanoic acid, zinc salt; UNII-H92E6QA4FV; A830766; XOOUIPVCVHRTMJ-UHFFFAOYSA-L; Stearic acid, zinc salt;

Smiles: CCCCCCCCCCCCCCCCCC(=O)[O-].CCCCCCCCCCCCCCCCCC(=O)[O-].[Zn+2];

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Molecular Weight 630.457 g/mol630.457 g/mol"Exact Mass" - Based on Specific Isotopes
 630.457 g/mol630.457 g/molMonoisotopic Mass - Isotopic Peak from Most Abundant Isotopes
 632.332 g/mol632.332 g/mol
Vapor Pressure 0.000 bar0.000 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °F
 
Descriptive Properties
Alfa Chemistry Materials CategoryPolymer Science
CAS Number557-05-1
Color/FormWhite powder free from grittiness; Fine, soft, bulky powder;
Complexity196
Covalently-Bonded Unit3
DecompositionDecomposes on burning producing irritating and toxic fumes including zinc oxide.
EC Number209-151-9
H-Bond Acceptor4
Heavy Atom Count41
ICSC Number0987
InChIInChI=1S/2C18H36O2.Zn/c2*1-2-3-4-5-6-7-8-9-10-11-12-13-14-15-16-17-18(19)20;/h2*2-17H2,1H3,(H,19,20);/q;;+2/p-2;
InChIKeyXOOUIPVCVHRTMJ-UHFFFAOYSA-L;
IUPAC Namezinc;octadecanoate;
Molecular FormulaC36H70O4Zn or C36H70O4Zn
Octanol/Water Partition Coefficient1.2;
OdorSlight, characteristic odor
Other PropertiesDecomp by dilute acids; Hydrophobic
pHNeutral to moistened litmus paper;
Rotatable Bond Count30
RTECS NumberZH5200000
StorageStable; store in a well-closed container in a cool, dry place
Topological Polar Surface Area80.3A^2
UN Number3077
UNIIH92E6QA4FV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA2572 / 268839

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.