MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dioshy UL-860KM SEBS Specialized Series
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Features:
  • Specialized grades, except silicone and rubber touch, including other special properties: shock absorbent, electric conductivity or wood-like appearance.
  • GP-XXXCN-1standard series, excellent anti-shock property, absorbed shocking energy to achieve the real shock resistance.
  • FP series can be applied for foaming application alone, to gain softer products (Shore C 13); also can be blended with EVA or PE for fine tuning the hardness.
  • HG standard series, electric conduction grades; can be classified into anti-static 106~109 or 107~1011; electric conduction 103~106 and super high electric conductivity 500O (102).
  • SP series can be classified into natural wood powder or natural cork powder; unique appearance and touch feeling.
  • Green material, passed heavy metal regulation, RoHS and EACH –SVHC

Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.297 g/cc1.297 g/ccJIS-K6301
Melt Flow 6.66 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.66 g/10 min
@Load 4.76 lb,
Temperature 374 °F
JIS-K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060JIS-K6301
Tensile Strength 4.02 MPa583 psi
Elongation at Break 739 %739 %JIS-K6310
100% Modulus 1.18 MPa171 psiJIS-K6310
300% Modulus 0.490 MPa71.1 psiJIS-K6310
Tear Strength 169 kN/m963 pliJIS-K6310-B
Compression Set 16 %
@Temperature 23.0 °C,
Time 79200 sec
16 %
@Temperature 73.4 °F,
Time 22.0 hour
JIS-K6301
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 180 °C338 - 356 °FInjection
Middle Barrel Temperature 175 - 185 °C347 - 365 °FInjection
Front Barrel Temperature 185 - 195 °C365 - 383 °FInjection
Nozzle Temperature 195 - 230 °C383 - 446 °FInjection
Drying Temperature 85.0 °C185 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
ApplicationUL94-V0
ColorWhite
TPS typeSEBS-O

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIOSH027 / 294637

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.