MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Carbon Printers SIL 30 Silicone Urethane Elastomer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Silicone

Material Notes: SIL 30 is a soft, biocompatible, and tear resistant silicone urethane elastomer that is ideal for comfortable skin-contact applications.

Information provided by Carbon®

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³liquid resin
 1.07 g/cc0.0387 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535instant; ASTM D2240
 31
@Time 5.00 sec
31
@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 3.20 MPa464 psiDie-C Shape, 500 mm/min; ASTM D412
Tensile Stress  0.420 MPa
@Strain 50 %
60.9 psi
@Strain 50 %
Die-C Shape, 500 mm/min; ASTM D412
 0.690 MPa
@Strain 100 %
100 psi
@Strain 100 %
Die-C Shape, 500 mm/min; ASTM D412
 1.45 MPa
@Strain 200 %
210 psi
@Strain 200 %
Die-C Shape, 500 mm/min; ASTM D412
Elongation at Break >= 330 %>= 330 %Die-C Shape, 500 mm/min; ASTM D412
Resilience 2020[%], Bayshore Rebound; ASTM D2632
Tear Strength 9.60 kN/m54.8 pliDie-C (die cut); ASTM D624
Compression Set 11 %
@Temperature 23.0 °C,
Time 259000 sec
11 %
@Temperature 73.4 °F,
Time 72.0 hour
ASTM D395-B
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 7.6
@Frequency 1e+6 Hz
7.6
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.15
@Frequency 1e+6 Hz
0.15
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 8.00 °C46.4 °FDMA, tan(d); ASTM D4065

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCARBP011 / 255843

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.