MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped rolled up and sealed in a plastic bag to preserve its moldability.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.460 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 0.480 MPa
Compressive Yield Strength 0.200 MPaat 10% Compression
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0600 W/m-K
@Temperature 200 °C
ASTM C177
 0.130 W/m-K
@Temperature 500 °C
ASTM C177
 0.200 W/m-K
@Temperature 800 °C
ASTM C177
Maximum Service Temperature, Air 1260 °C
Shrinkage 0.00 %
@Temperature 75.0 °C
Drying
 2.0 %
@Temperature 800 °C,
Time 86400 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 66 %
SiO2 34 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites Alumina Coat
Zircar Refractory Composites RS-200 Refractory Sheet
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet

CZRCI07 / 2870

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.