MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos Mecoline IS RDX 5242 F Radiation cross-linkable PVDF flame retardant
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable PVDF flame retardant

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: Halogenated

Standards: NEMA WC 27500; SAE AS 81044/9; SAE AS 81044/12

Typical applications: This compound is an excellent choice for manufacturing insulated hook-up wires in military and aerospace industries (airframe wire) and component conductors for NEMA WC 27500 cables.

Features: Flame retardant; Low smoke; Oil resistant; Abrasion resistant; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³pressed plaques; DIN EN ISO 1183-1A
Melt Flow 42 g/10 min
@Load 21.6 kg,
Temperature 230 °C
42 g/10 min
@Load 47.6 lb,
Temperature 446 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565pressed plaques; DIN ISO 7619-1
Tensile Strength >= 25.0 MPa>= 3630 psicross-linked plaques or tapes, 70-80kGy; IEC 60811-501
Elongation at Break >= 175 %>= 175 %cross-linked plaques or tapes, 70-80kGy; IEC 60811-501
 >= 125 %
@Temperature 200 °C,
Time 605000 sec
>= 125 %
@Temperature 392 °F,
Time 168 hour
cross-linked plaques / tapes, After ageing in air oven; IEC 60811-401
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+11 ohm-cm>= 1.00e+11 ohm-cmpressed plaques; ASTM D 257
Dielectric Strength >= 15.0 kV/mm>= 381 kV/inpressed plaques; ASTM D 2671
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94 V-0V-0pressed plaques
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 230 °C428 - 446 °FTool
 250 °C482 °FMaximum mass temperature
Zone 1 180 - 190 °C356 - 374 °F
Zone 2 190 - 200 °C374 - 392 °F
Zone 3 200 - 210 °C392 - 410 °F
Zone 4 210 - 220 °C410 - 428 °F
Zone 5 210 - 220 °C410 - 428 °F
Adapter Temperature 220 - 230 °C428 - 446 °F
Head Temperature 220 - 230 °C428 - 446 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 42 %42 %pressed plaques; ASTM D 2863 A
 
Descriptive Properties
Heat shockNo cracks4h at 250°C, ASTM D 2671
Water absorption0.5 mg/cm³after 24h at 23°C, ASTM D-570

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS046 / 296153

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.