MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient Lubri-Tech™ NN-30GF/13T/2S Nylon 6/6, Glass Filled, PTFE/Silicone Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

Description/Features:

  • Glass Fiber Reinforced
  • PTFE/Silicone Lubricated

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Water Absorption 0.50 %
@Thickness 3.17 mm
24 hr. Immersion; ASTM D570
Water Absorption at Saturation 2.5 %
@Thickness 3.17 mm
Long-Term Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 24000 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 1.20e+6 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 30000 psiASTM D790
Flexural Modulus 1095 ksiASTM D790
Compressive Strength 20000 psiASTM D695
Shear Strength 9500 psiASTM D732
Izod Impact, Notched 1.80 ft-lb/in
@Thickness 6.35 mm,
Temperature 23.0 °C
Method A, Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 500 °FUnannealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 490 °FUnannealed, 0.125 in bars; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Lubri-Tech™ NN-30GF/15KV5T UV HS Nylon 6/6, Glass Filled, PTFE Lubricated
RTP Company RTP 207 TFE 13  Nylon 6/6 (PA 6/6) Glass Fiber 40% - PTFE 13% - Silicone 2%
RTP Company RTP 205 TFE 13 SI  Nylon 6/6 (PA 6/6) Glass Fiber 30% - PTFE 13% - Silicone
RTP Company RTP 201.3 TFE 10 SI 2  Nylon 6/6 (PA 6/6) Glass Fiber 13% - PTFE 10% - Silicone 2%
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone

PH1PO0334 / 43490

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.