MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® L2141 BK 9.750 Nylon 12, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® L2141 BK 9.7504 is a heatstabilized polyamide 12 compound for the extrusion of tubing (e.g. fuel lines) and semi-finished products. Tubing according to DIN 73 378, Type: PA 12-HL. Properties of compounds based on PA12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Lubricant, Unfilled
Processing: Profile extrusion
Special Characteristics: High heat resistant, High viscosity
Color: Black
Additives: Light stabilizer, Heat stabilizer, Processing aids

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psiISO 527
Elongation at Break >= 50.0 %>= 50.0 %Nominal; ISO 527
Elongation at Yield 12.0 %12.0 %ISO 527
Tensile Modulus 1.30 GPa189 ksiISO 527
Flexural Strength 35.0 MPa5080 psiat conv. Deflection; ISO 178
 46.0 MPa6670 psiISO 178
Flexural Modulus 1.08 GPa157 ksiISO 178
Flexural Strain at Break 8.00 %8.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+10 ohm-cm5.00e+10 ohm-cmIEC 62631-3-1
Surface Resistance 6.00e+14 ohm6.00e+14 ohmIEC 62631-3-2
Dielectric Constant  3.50
@Frequency 1.00e+6 Hz
3.50
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 5.00
@Frequency 100 Hz
5.00
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 35.0 kV/mm889 kV/inAC, S20/S20, t.; IEC 60243-1
Dissipation Factor  0.0500
@Frequency 1.00e+6 Hz
0.0500
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.110
@Frequency 100 Hz
0.110
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Injection Pressure 70.0 MPa10200 psiInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption26.1 kgISO 14040, 14044
ColorBlack
Flexural stress at breakNMPa, ISO 178
 N%, ISO 178
Global Warming Potential2.7 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.8 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7909 / 325041

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.