- Bullet Resistant Material
- UL® Recognized
- UL-752 Levels 1-5, and 8 Outdoor Rating
- UL-94 V0 Flame Rating
- Lightweight
- Military and Commercial Applications
DuroProtect® is a thin and lightweight composite panel that has been recognized by Underwriters Laboratories to meet their UL-752 specifications for bullet resisting plastics. (Levels 1-5 and 8). DuroProtect® has been rated to stop threats form a multitude of firearms tested in various conditions and shot patterns at short range. DuroProtect® is designed to provide protection from bullets and other projectiles. DuroProtect® can be used in a variety of applications where personal and property protection is required or desired. Threat level 4,5 and 8 panels can be achieved by bonding a combination of the other threat levels together or can be molded to thickness. Both were tested and meet the requirements of UL-752.Applications: - Government Buildings
- Drive-up Bank Tellers
- ATM’s
- Guard Houses
- Safe Rooms
- Vehicle Armor
- Schools/Classrooms
- Window Shutters/Storm Shelters
- Convenience Stores
- Gas Stations
- Courtrooms
- Toll Booths
- Others
Information provided by Röchling. |