MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

n-Tetradecane, C14H30
Categories: Fluid; Solvent

Key Words: C14H30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.763 g/cc
@Temperature 20.0 °C
0.0276 lb/in³
@Temperature 68.0 °F
Viscosity 10.822 cP
@Temperature 20.0 °C
10.822 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 198.394 g/mol198.394 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 16.2 bar12200 torr
Critical Temperature 421 °C790 °F
Critical Density 0.239 g/cc0.00863 lb/in³
Critical Molar Volume 830 cm³/mol50.6 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 238.8 J/g102.7 BTU/lb
Thermal Conductivity 0.1363 W/m-K
@Temperature 20.0 °C
0.9459 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 5.90 °C42.6 °F
Boiling Point 253.6 °C488.5 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter311.21
Antoine's Vapor Pressure B Parameter-79.38
Antoine's Vapor Pressure C Parameter15.97
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)629-59-4
Chemical FormulaC14H30
Critical Compressibility (Zc)0.23
Molar Heat Capacity (298K)J/mol-K
Molar Heat Capacity of Vapor a Parameter-10.9746
Molar Heat Capacity of Vapor b Parameter13.3679
Molar Heat Capacity of Vapor c Parameter-4.184
Molar Heat Capacity of Vapor d Parameter-7.418
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VORGS328 / 99680

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.